Polymer Property : Izod Impact Unnotched = 24.4 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Unnotched 24.4 J
18.0 ft-lb
Air Cooled from 788°C; 94°C Temper Temperature
Latrobe Graph-Air® Cold Work Tool Steel (ASTM A10)
Graph-Air tool steel is an air-hardening, graphitic tool steel with outstanding resistance to metal-to-metal sliding wear and galling. The steel contains a uniform dispersion of graphite particles w..
Izod Impact Unnotched 24.4 J
18.0 ft-lb
Air Cooled from 1010°C; As Quenched
Latrobe LSSâ„¢ D7 Tool Steel (ASTM D7)
TLS D7 tool steel is a high-carbon, high-chromium air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide ..
Izod Impact Unnotched 24.4 J
18.0 ft-lb
Oil Quenched at 1191°C; 622°C Temper Temperature
Latrobe Dynamax™ ASTM M42, DIN 1.3247 Super High Speed Steel
Dynamax super high speed steel is a premium cobalt high speed steel with a chemical composition designed for high hardness and superior hot hardness. These properties make the steel an excellent cho..