Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 39.2 - 49.0 MPa | 5690 - 7110 psi | Cold Crushing |
Sharadaa Ceramics HH 42SD Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 39.2 - 49.0 MPa | 5690 - 7110 psi | Cold Crushing |
Sharadaa Ceramics HH 45D Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |