Mechanical Properties Metric English Comments
Compressive Strength 2230 - 2430 MPa
323000 - 352000 psi
Rc0.2; varies with tempering. This range is for HRC between 58 and 61.
Bohler-Uddeholm UDDEHOLM Caldie Plastic Mold Tool Steel
Description: Uddeholm Caldie is a chromium-molybdenumvanadium alloyed tool steel.Uddeholm Caldie which is characterized by:Very good chipping and cracking resistanceGood wear resistanceHigh hardness..