Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® 160 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® 106 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Compressive Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Abatron AboCast 7802-1/AboCure 50-3 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, ..
Compressive Strength 13.8 - 20.7 MPa
2000 - 3000 psi
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy
AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia..
Compressive Strength 13.8 - 20.7 MPa
2000 - 3000 psi
ASTM D695
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Compressive Strength 10.3 - 20.7 MPa
1500 - 3000 psi
Crush Strength
Trelleborg Fillite® PG (300LF) Alumino-silicate Cenospheres