Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 100 - 150 MPa | 14500 - 21800 psi | Injection; ISO 604 |
Raschig Group 2572 AMC Glass fiber reinforced Polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, good abrasion stability, high flame retardance in combin.. |
|||
Compressive Strength | 100 - 150 MPa | 14500 - 21800 psi | ISO 604 |
Raschig Group DECAL® 937 Phenolic Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W.. |
|||
Compressive Strength | 60.0 - 150 MPa | 8700 - 21800 psi | Perpendicular to Plane |
Goodfellow Carbon-Carbon Composite Carbon Fiber - Carbon MatrixInformation provided by Goodfellow. |