Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 64.3 MPa | 9320 psi | ASTM C579 |
Chesterton ARC 791 Composite Description: A quartz reinforced composite designed to resurface and restore concrete surfaces, to protect new concrete, and to repair concrete damaged by chemical and physical abuse. ARC 791 has ex.. |