Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 570 MPa | 82700 psi | Longitudinal |
Goodfellow Carbon/Epoxy Composite Sheet Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Compressive Strength | 570 MPa | 82700 psi | Transverse |
Goodfellow Carbon/Epoxy Composite Sheet Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |
|||
Compressive Strength | 570 MPa @Treatment Temp. 20.0 °C, Time 3600 sec |
82700 psi @Treatment Temp. 68.0 °F, Time 1.00 hour |
ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Compressive Strength | 570 MPa @Temperature 23.0 °C |
82700 psi @Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 4011 Polyimide, Yellow (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |