Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 550 MPa | 79800 psi | |
ICE Steatite L-4 Data provided by the manufacturer, International Ceramic Engineering. |
|||
Compressive Strength | 550 MPa | 79800 psi | ASTM C773 |
CoorsTek Mullite, S2 Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Compressive Strength | 550 MPa @Thickness >=5.00 mm |
79800 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax EP 11 Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: High resistance to chemicals. Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic t.. |
|||
Compressive Strength | 550 MPa @Thickness >=5.00 mm |
79800 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax EP 215 S Epoxy, Glass Fabric Reinforcement, Green, Sheets Description: Particularly good, lasting strength properties and insulation values even at high application temperatures. Radiation-resistant. Can be used at cryogenic temperatures. Very good where t.. |
|||
Compressive Strength | 550 MPa @Thickness >=5.00 mm |
79800 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. UL-94 V.. |
|||
Compressive Strength | 550 MPa @Thickness >=5.00 mm |
79800 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax EP 10 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c.. |
|||
Compressive Strength | 550 MPa @Thickness >=5.00 mm |
79800 psi @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3 |
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets Description: High mechanical strength at elevated temperatures. Very good stability of electrical properties under high humidity. Mechanical, electrical and electronic applications. Can be used at c.. |