Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | <= 0.490 MPa | <= 71.1 psi | Cold Crushing Strength |
Chosun Refractories A-2 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 0.490 MPa | <= 71.1 psi | Cold Crushing Strength |
Chosun Refractories A-3 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 0.490 MPa | <= 71.1 psi | Cold Crushing Strength |
Chosun Refractories A-1 Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |