Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 48.3 MPa | 7000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Fluorosint® 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers (ASTM Product Data Sheet) Chemical resistance parallels PTFE Continuous use temperatures to 500°F (260°C) Compared to PTFE higher load carrying capability 1/9 of the deformation under load lower coefficient of thermal exp.. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | ASTM D695 |
ScanTube ECTFE Tubing Information provided by ScanTube, Inc. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | ASTM D695 |
ScanTube ETFE Tubing Information provided by ScanTube, Inc. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | ASTM-C773 |
CoorsTek PolyGlyde™ 5400 Self-Lubricating Seal PolyGlyde seals offer low heat generation in high-friction and high-stress environments. These seals provide superior performance over traditional carbon materials: runs cooler – even in dry-runni.. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | |
Cotronics Resbond™ 903HP High Temperature Ceramic Adhesive, Hi-Bond Strength |
|||
Compressive Strength | 48.3 - 207 MPa | 7000 - 30000 psi | |
Du-Co Ceramics S-470 Aluminum Silicate Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Compressive Strength | 48.3 - 207 MPa | 7000 - 30000 psi | |
Du-Co Ceramics S-699 Alumina Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | |
Aremco Ceramacast™ 645-N High Temperature Potting & Casting Material Silica Castable ceramic with low thermal conductivity. |
|||
Compressive Strength | 48.3 - 55.2 MPa | 7000 - 8000 psi | |
Abatron AboCast 7802-1/AboCure 50-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-3 is a clear, slow converter for lower rigidity. It has an HDT of 60°C, variable ratio, .. |
|||
Compressive Strength | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Abatron AboCast 7802-1/AboCure 7804-3 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Compressive Strength | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
Abatron AboCast 7802-1/AboCure 7804-4 (40 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Compressive Strength | 48.26 - 62.05 MPa | 7000 - 9000 psi | after 816°C |
Pyrotek Pyrocast ZS Refractory Shapes Aggregate Base: Fused SilicaApplicationsTransfer troughs Information provided by Pyrotek. |
|||
Compressive Strength | 48.3 MPa | 7000 psi | Break; TM R050-38 |
Resinlab® EP1296 Highly Filled, Moderately Thixotropic Black Casting Resin Resinlab™ EP1296 is a highly filled, moderately thixotropic black casting resin designed for applications requiring good thermal conductivity, low shrinkage and a low CTE. It was especially formula.. |