Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 448 MPa @Temperature 23.9 °C |
65000 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-766B Epoxy Prepreg, 7581 E-Glass Reinforced Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.Key Features and Benefits:Self adhesive resin system f.. |
|||
Compressive Strength | 448 MPa @Temperature 23.9 °C |
65000 psi @Temperature 75.0 °F |
Dry; 325°F Autoclave Cured; ASTM D695 |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Compressive Strength | 448 MPa @Temperature 23.9 °C |
65000 psi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® F-562 Phenolic Prepreg, 8HS Silica Reinforced Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environm.. |
|||
Compressive Strength | 448 MPa @Temperature 82.2 °C |
65000 psi @Temperature 180 °F |
Wet; ASTM D695 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Compressive Strength | 448 MPa | 65000 psi | |
Pyrotek TS-105 Thermoset Electrical Insulation Product (Nema Grade: G-5) Glass reinforcement, Melamine Resin, Gray color. High mechanical strength, arc and heat resistance. Self-extinguishing.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulat.. |
|||
Compressive Strength | 448 MPa | 65000 psi | |
Pyrotek TS-109 Thermoset Electrical Insulation Product (Nema Grade: G-9) Glass reinforcement, Melamine Resin, Gray color. High mechanical strength, arc and heat resistance. Self-extinguishing.Information provided by Pyrotek. |
|||
Compressive Strength | 448 MPa | 65000 psi | |
Pyrotek TS-206 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Dark Red color. High compressive and flexural strength.Information provided by Pyrotek. |
|||
Compressive Strength | 448 MPa | 65000 psi | ASTM D695 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Compressive Strength | 448 MPa | 65000 psi | ASTM D695 |
G-9 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane.. |
|||
Compressive Strength | 448 MPa | 65000 psi | ASTM D695 |
G-5 Fiberglass Melamine Laminate Sheet This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and .. |