Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0434 MPa | 6.30 psi | Force to Compress, 50% compression; Norton Test Procedure 10 |
Saint-Gobain Norton® Log Home Foam® V790 Description: Provides Positive Seal in Log Home Joints: Norseal® Log Home Foam® V790 is a medium-density foam specifically developed for log home gasketing. Under a minimum of 25 percent compr.. |