Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 367 MPa | 53200 psi | Typical |
Magnesium Elektron Elektron® 21 Magnesium Casting Alloy Fully heat treatable alloy for use up to 400°F. Excellent corrosion resistance and castability. Cast products possess a fine-grained microstructure and pressure tightness. Easily machined. Usual .. |