Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 303 MPa | 43900 psi | |
Pyrotek TS-82 Thermoset Electrical Insulation Product (Nema Grade: XXX) Paper reinforcement, Phenolic Resin, Natural Color. High humidity resistance, Excellent resistance to splitting.Information provided by Pyrotek. |
|||
Compressive Strength | 303 MPa | 43900 psi | |
Haysite HCR-197 Corrosion Resistant Polyester/Glass Sheet A fiber glass reinforced thermoset polyester sheet using ATLAC® 382 Bisphenol-A Fumarate in the resin matrix. Standard color is light yellow. Additional data covering resistance to specific chemi.. |