Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 290 MPa | 42100 psi | Flatwise; ASTM D695 |
Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3) Data provided by Glastic Corporation.NEMA GPO-3. Average data - may vary with the size and shape of the electrical insulating structural product. |