Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 26.2 MPa | 3800 psi | 10% Def.; ASTM D695 |
Quadrant EPP Fluorosint® 207 PTFE, Compression Molded Synthetic Mica-filled PTFE (ASTM Product Data Sheet) |
|||
Compressive Strength | 26.2 MPa | 3800 psi | 10% Def.; ASTM D695 |
Quadrant EPP PROTEUS® EURO-GRAY Copolymer Polypropylene |
|||
Compressive Strength | 26.2 MPa | 3800 psi | ASTM D695 |
Greene Tweed Avalon® 16 PTFE, Glass, Molybdenum Filled Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
Compressive Strength | 26.2 MPa | 3800 psi | |
Henkel Hysol EA 9396.6MD Paste Adhesive System Cure syntactic, with excellent high temperature properties. Applications: Potting Syntactic |
|||
Compressive Strength | 26.2 MPa | 3800 psi | 10% Def.; ASTM D695 |
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet) |