Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2600 MPa | 377000 psi | |
Sapco 98% Aluminum Oxide Information provided by Sapco. |
|||
Compressive Strength | 2600 MPa | 377000 psi | ASTM C773 |
CoorsTek AD-995 Alumina (nom. 99.5% Al2O3) Thermal Shock Delta Tc = 200°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Compressive Strength | 2600 MPa | 377000 psi | ASTM-C773 |
CoorsTek AD-996 99.6% Alumina |
|||
Compressive Strength | 2600 MPa | 377000 psi | ASTM-C773 |
CoorsTek CAP 3 99.5% Alumina Ceramic Armor Material CoorsTek CeraShield™ ceramics provide: low weight, high hardness, controlled, uniform microstructure, dimensional stability over wide temperature range, compatibility for use in finished armor sys.. |