Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 257 MPa | 37300 psi | ISO 604 |
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by .. |