Mechanical Properties Metric English Comments
Compressive Strength 2450 MPa
355000 psi
ASTM-C773
CoorsTek ADD-96 96% Alumina
Compressive Strength 2450 MPa
355000 psi
HRC 55 R<sub>cm</sub>
Assab Steels DF-3 Cold Work Steel
DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil..