Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 226 MPa | 32800 psi | ASTM D695 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |