Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 20.3 MPa | 2950 psi | |
TriStar TriSteel PT Metal Backed PTFE Bearing System Ultraflon 602 (PT) PTFE lined metal backed bearing system, low friction, high PV, high speed sleeve, flange and thrust bearings, zero lube required, high operating temperature. Ultraflon 602 PTFE Li.. |