Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 19.6 MPa | 2840 psi | Cold Crushing |
Sharadaa Ceramics HH 40 Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 19.6 - 24.5 MPa | 2840 - 3560 psi | Cold Crushing |
Sharadaa Ceramics HH 42 Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | 19.6 MPa | 2840 psi | Cold Crushing |
Sharadaa Ceramics MH 30 Normal Medium and High Heat and Super Duty Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Compressive Strength | <= 19.6 MPa | <= 2840 psi | Cold Crushing Strength |
Chosun Refractories BATN-3 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 19.6 MPa | <= 2840 psi | Cold Crushing Strength |
Chosun Refractories BATN-8 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 19.6 MPa | <= 2840 psi | Cold Crushing Strength |
Chosun Refractories BATN-D2, Lower Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 19.6 MPa | <= 2840 psi | Cold Crushing Strength |
Chosun Refractories BATN-D2, Upper Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 19.6 MPa | <= 2840 psi | Cold Crushing Strength |
Chosun Refractories BP-95A Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 19.6 MPa | <= 2840 psi | Cold Crushing Strength |
Chosun Refractories BPR-S Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 19.6 MPa | <= 2840 psi | Cold Crushing Strength |
Chosun Refractories BTN-2 Gas Purging Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | <= 19.6 MPa | <= 2840 psi | Cold Crushing Strength |
Chosun Refractories IC-RK Special Insulating Firebrick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 - 29.4 MPa @Temperature 1500 °C, Time 10800 sec |
2840 - 4270 psi @Temperature 2730 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TAST-170 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Compressive Strength | 19.6 MPa | 2840 psi | Cold Crushing Strength |
Chosun Refractories ALB-65I Special Casting Block Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |