Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 186 MPa | 27000 psi | |
Poco Graphite ACF-10Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
Compressive Strength | 186 MPa | 27000 psi | Ultimate |
Resinlab® EP691 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP 691 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting.. |
|||
Compressive Strength | 186 MPa | 27000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet) |
|||
Compressive Strength | 186 MPa | 27000 psi | 10% Deformation; ASTM D695 |
Quadrant EPP Duratron® PI D7000 PI Unfilled Polyimide (ASTM Product Data Sheet) |
|||
Compressive Strength | 186 MPa | 27000 psi | ASTM D695 |
IDI Composites C-105 Thermoset Polyester, Molding Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer. |
|||
Compressive Strength | 186 MPa | 27000 psi | ASTM D695 |
IDI Composites C-204 Thermoset Polyester, Sheet CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by .. |
|||
Compressive Strength | 186 MPa | 27000 psi | ASTM D695 |
IDI Composites E-204 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Compressive Strength | 186 MPa @Thickness 12.7 mm |
27000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP612 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require.. |
|||
Compressive Strength | 186 MPa | 27000 psi | ASTM D695 |
Sumitomo Bakelite Durez® 153 Phenolic, Injection Grade Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a.. |
|||
Compressive Strength | 186 MPa | 27000 psi | ASTM D695 |
Sumitomo Bakelite North America RX® 431 Cellulose Reinforced Phenolic Novolac RX431 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Compressive Strength | 186 MPa | 27000 psi | |
Cosmic Plastics 6130F Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 186 MPa | 27000 psi | |
Cosmic Plastics 6230 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 186 MPa | 27000 psi | ASTM D695 |
Plenco 4349 Phenolic, Granular, Injection Molded PLENCO 04349 is a heat resistant, mineral filled phenolic molding compound offering optimized cure characteristics, and excellent heat resistant properties. PLENCO 04349 is also formulated to offer .. |
|||
Compressive Strength | 186 MPa | 27000 psi | |
Cosmic Plastics K61 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 186 MPa | 27000 psi | |
Cosmic Plastics K66 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 186 MPa | 27000 psi | ASTM D695 |
Plenco 4311 Phenolic, Granular, Compression Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
Compressive Strength | 186 MPa | 27000 psi | |
Cosmic Plastics D69 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 186 MPa | 27000 psi | |
Cosmic Plastics D62 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 186 MPa | 27000 psi | |
Cosmic Plastics 6130 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 186 MPa | 27000 psi | |
Cosmic Plastics 6230F Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 186 - 214 MPa | 27000 - 31000 psi | |
Bulk Molding Compounds BMC T45HT Automotive Grade Molding compound BMC T45HT was designed for the very demanding applications of automotive under hood engine covers. It meets the GMP UP .007 specification for automotive under hood. BMC T45HT is a vinyl ester base.. |