Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
Premix Premi-Glas® 1200-20 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-20 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
Premix Premi-Glas® 1200H-20 Polyester SMC Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
Premix Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
Premix Premi-Glas® 1240-20 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-20 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Compressive Strength | 165 MPa | 23900 psi | Test specimen flat tested; ISO 604 |
Hexion Bakelite™ X65 Phenolic Formaldehyde Resin, UL Listed
(discontinued **) Phenolic molding compound, inorganically/organically filled, good heat-resistance and dimensional stability, UL listed molding compound 3.0 mm/V-0 (BN, BK).Application areas: Oven strips.Information.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
IDI Composites 48-50 Thermoset Polyester, Molding Moderate strength electrical grade with good track resistance and V-O flame resistance.Data provided by the manufacturer. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
IDI Composites A-203 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
IDI Composites C-103 Thermoset Polyester, Molding Vinylester compounds in a range of strengths with superior corrosion resistance.Data provided by the manufacturer. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
IDI Composites E-203 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
IDI Composites M-203 Thermoset Polyester, Sheet MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
Plenco 2369 Phenolic, Granular, Compression Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Compressive Strength | 165 MPa | 23900 psi | |
Cosmic Plastics 306 Orlon Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
Plenco 4309 Phenolic, Nodular, Injection Molded PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430.. |
|||
Compressive Strength | 165 MPa | 23900 psi | |
Cosmic Plastics D45 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Compressive Strength | 165 MPa | 23900 psi | Test specimen flat tested; ISO 604 |
Hexion Bakelite™ PF 8052 Phenolic Formaldehyde Resin, Resistant to High Temperatures
(discontinued **) Phenolic molding compound, glass fiber reinforced and inorganically filled. Excellent heat resistance with respect to surface finish and mechanical properties.Application areas: Pan handles, heat r.. |
|||
Compressive Strength | 165 MPa | 23900 psi | ASTM D695 |
Sumitomo Bakelite North America FM 7700P Fiberglass and Mineral Reinforced Phenolic Novolac FM 7700P is a two-stage phenolic molding compound reinforced with cotton fabric in pellet form. FM-7700P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-20. (Replaces Mil.. |
|||
Compressive Strength | 165 MPa | 23900 psi | |
Cosmic Plastics D44 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |