Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 16.0 MPa | 2320 psi | 1% strain over 1000 hours; ISO.899 DIN.53444 |
Omnia Plastica Noryl® PPO m Polyphenylenoxide Noryl is a resin based on polyphenylene oxide, modified with styrene. Its main field of application is the electrical one.Features:Good electrical properties, even at high frequency Dimensional stab.. |
|||
Compressive Strength | 16.0 MPa | 2320 psi | |
Pyrotek Pyrite N-17 Refractory Board Pyrotek N-17 is a graphite fiber reinforced, high purity, calcium silicate board developed exclusively for the non-ferrous casting industry. The patented formulation of Pyrotek N-17 makes it good i.. |
|||
Compressive Strength | 16.0 MPa | 2320 psi | 5% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 700 Ultra High Molecular Weight Polyethylene Application: wear liners, sliding platesInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 16.0 MPa | 2320 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Compressive Strength | 16.0 MPa @Strain 3.50 % |
2320 psi @Strain 3.50 % |
DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Compressive Strength | >= 16.0 MPa | >= 2320 psi | |
Beijing Evergrow Resources PTFE, 15% Carbon Fiber Filled Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with fillers of many different kinds. Amongst the m.. |
|||
Compressive Strength | >= 16.0 MPa | >= 2320 psi | |
Beijing Evergrow Resources PTFE, 20% Glass Fiber Filled Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with fillers of many different kinds. Amongst the m.. |
|||
Compressive Strength | >= 16.0 MPa | >= 2320 psi | |
Beijing Evergrow Resources PTFE, 20% Glass Fiber, 5% Graphite Filled Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with fillers of many different kinds. Broadly speak.. |
|||
Compressive Strength | >= 16.0 MPa | >= 2320 psi | |
Beijing Evergrow Resources PTFE, 24% Bronze, 12% Glass Fiber, 6% Graphite Filled Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with filler. Broadly speaking PTFE compounds have t.. |
|||
Compressive Strength | >= 16.0 MPa | >= 2320 psi | |
Beijing Evergrow Resources PTFE, 25% Glass Fiber Filled Filled PTFE article is manufactured by molding method with filled PTFE resin. Filled PTFE resin is manufactured by compounding PTFE granular resin with filler. Broadly speaking PTFE compounds have t.. |