Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 138 MPa | 20000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Ketron® 1000 PEEK, Extruded Unfilled Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Compressive Strength | 138 MPa @Strain 10.0 %, Temperature 22.8 °C |
20000 psi @Strain 10.0 %, Temperature 73.0 °F |
ASTM D732 |
Quadrant EPP Ketron® HPV PEEK High Pressure Velocity Polyetherether Ketone (ASTM Product Data Sheet) This bearing grade of extruded Ketron PEEK offers the lowest coefficient of friction and best machinability of all Ketron grades. It is ideal for low wear, high PV parts that require chemical resis.. |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1385 Black Epoxy Formulation Resinlab™ EP1385 Black is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Break; TM R050-38 |
Resinlab® EP1385 Clear Epoxy Formulation Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Compressive Strength | 138 MPa | 20000 psi | |
Poco Graphite DFP-3-2 Ion Implant Grade Graphite This is a high strength graphite that has reduced porosity. DFP-3-2 has long been the standard for components that exhibit long life and reduced erosion rates. |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
Technetics Group Amicon™ PEEK
(Unverified Data**) Information provided by Technetics Group (formerly Plastomer Technologies) |
|||
Compressive Strength | 138 MPa | 20000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Duratron® PAI T4540 Polyamide-imide, compression molded (ASTM Product Data Sheet) |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not only.. |
|||
Compressive Strength | 138 - 152 MPa | 20000 - 22000 psi | ASTM D695 |
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Compressive Strength | 138 - 165 MPa | 20000 - 24000 psi | ASTM D695 |
Mar-Bal MB2000-20 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Compressive Strength | 138 MPa | 20000 psi | |
Glastic 4640-15 Fiberglass-Reinforced Polyester Standoff Insulator Glastic Standoff Insulators are molded of UL recognized flame resistant fiberglass-reinforced thermoset polyester molding compound. They feature shatter resistance and closer height tolerances than.. |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4435 Polyamide-imide (PAI) Torlon® 4435 is a polyamide-imide resin specifically designed to provide exceptionally low wear performance in non-lubricated applications even at high pressure and velocity (PV) conditions. Not .. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond EP112FLAO-1 Toughened, Two component, Heat Curing Epoxy Master Bond EP112FLAO-1 is a toughened two component, high performance epoxy resin system featuring very good temperature resistance, fine thermal conductivity and electrical insulation values with .. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond EP17HT One component epoxy system for bonding, sealing, coating and casting Product Description: Master Bond EP17HT is an one component, heat cured epoxy system for bonding, sealing, coating and encapsulating. It features good physical properties, electrical insulation prof.. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
Compressive Strength | >= 138 MPa | >= 20000 psi | |
Master Bond Ep46HT-2 Two Component, Heat Resistant Epoxy System Master Bond Polymer System EP46HT-2 is a two component epoxy system for bonding, sealing and casting applications where resistance to temperatures from -100°F to +500°F is required. It is 100% rea.. |
|||
Compressive Strength | 138 - 165 MPa | 20000 - 24000 psi | |
Bulk Molding Compounds BMC 501 Mineral Filled, Glass Fiber Reinforced Compound BMC 501 molding compound is a mineral filled glass-fiber-reinforced compound suitable for compression, transfer and stuffer injection molding. It provides the user with good electrical properties An.. |
|||
Compressive Strength | 138 - 165 MPa | 20000 - 24000 psi | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Compressive Strength | 138 - 152 MPa | 20000 - 22000 psi | |
Bulk Molding Compounds BMC 1410 Electrical Grade BMC 1410 is a high-strength electrical grade material with excellent flammability resistance. In most applications, this material is competitive with SMC. Equal performance at a lower cost. Normally.. |
|||
Compressive Strength | 138 MPa | 20000 psi | ASTM D695 |
Quantum Nylon 6/6 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate .. |
|||
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1199 Black Unfilled Epoxy Adhesive Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Break; TM R050-38 |
Resinlab® EP1199 Black Unfilled Epoxy Adhesive Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Break; TM R050-38 |
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive Resinlab™ EP11HTFS Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Compressive Strength | 138 MPa | 20000 psi | Ultimate; TM R050-38 |
Resinlab® EP1290 Gray Mineral Filled Epoxy Adhesive Resinlab™ EP1290 Gray is a two part mineral filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-flexible material. It has good wetting to m.. |
|||
Compressive Strength | 138 - 165 MPa | 20000 - 24000 psi | |
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary. |
|||
Compressive Strength | 138 MPa | 20000 psi | Break; TM R050-38 |
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |