Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 12.73 MPa @Temperature 375 °C |
1846 psi @Temperature 707 °F |
|
Pyrotek Wollite 50 Insulating Castable Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c.. |