Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.117 - 0.172 MPa | 17.0 - 25.0 psi | Deflection @ 25%; ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C45 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.117 - 0.172 MPa | 17.0 - 25.0 psi | Deflection @ 25% |
Monmouth Rubber & Plastics Durafoamâ„¢ DK5151 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Compressive Strength | 0.117 MPa | 17.0 psi | at 25%, Horizontal; ASTM D3575, Suffix D |
Dow STRANDFOAM™ EA 1000 Polypropylene Foam STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra.. |
|||
Compressive Strength | 0.117 MPa | 17.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1215 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Compressive Strength | 0.117 MPa | 17.0 psi | 25% Compression, Deflection |
3M Cushion-Mount™ E1220 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |