Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 10.3 MPa | 1500 psi | Break; TM R050-38 |
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin.. |
|||
Compressive Strength | 10.3 - 20.7 MPa | 1500 - 3000 psi | Crush Strength |
Trelleborg Fillite® 160 Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Compressive Strength | 10.3 - 20.7 MPa | 1500 - 3000 psi | Crush Strength |
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Compressive Strength | 10.3 - 20.7 MPa | 1500 - 3000 psi | Crush Strength |
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Compressive Strength | 10.3 - 20.7 MPa | 1500 - 3000 psi | Crush Strength |
Trelleborg Fillite® 106 Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Compressive Strength | 10.3 - 20.7 MPa | 1500 - 3000 psi | Crush Strength |
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Compressive Strength | 10.3 - 20.7 MPa | 1500 - 3000 psi | Crush Strength |
Trelleborg Fillite® PG (300LF) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |