Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 7.79 - 7.86 MPa | 1130 - 1140 psi | |
BCC Products MB 1200 Polyurethane Foam Modeling Board MB 1200 is an Apricot and/or Pink colored rigid closed-cell polyurethane foam tooling and modeling board. MB 1200 is low density foam of approximately 20lbs/ft3 board. Easily cut using CNC machining.. |
|||
Compressive Strength | 7.80 MPa @Thickness 19.0 mm |
1130 psi @Thickness 0.750 in |
perpendicular to plane; ASTM C365 |
3A Composites Core Materials AIREX® PXc.385 Fiber-Reinforced Structural Foam AIREX® PXc is a closed-cell, fiber reinforced polymer foam with very high mechanical properties ideally suited as core material for structurally loaded sandwich applications. The sophisticated manu.. |