Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | ISO 604 |
Raschig Group 4552 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to +/- 300°C continuously, excellent electrical properties, good mechanical strength, very good dimensional stabi.. |
|||
Compressive Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | ISO 604 |
Raschig Group 4554 Silicone Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi.. |
|||
Compressive Strength | 70.0 MPa | 10200 psi | Cold Crushing Strength |
Gouda Vuurvast AK 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. In addition AK 60 A bricks have a very good slag resistance and high creep resistance (less than 0.2% .. |
|||
Compressive Strength | 70.0 MPa | 10200 psi | Cold Crushing Strength |
Gouda Vuurvast AK 80 A Dense Refractory Brick Description: A 78% alumina, bauxite based, quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from s.. |
|||
Compressive Strength | 70.0 MPa | 10200 psi | Cold Crushing Strength |
Gouda Vuurvast AK 80 AP Dense Refractory Brick Description: This phosphate bonded bauxite brick has an improved resistance against slag attack.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.. |
|||
Compressive Strength | 70.0 MPa | 10200 psi | Cold Crushing Strength |
Gouda Vuurvast AK 82 A Dense Refractory Brick Description: A high alumina bauxite based quality with a high abrasion resistance, therefore very well suitable for rotary cement kilns.Remarks: This data represents average values, obtained from sa.. |
|||
Compressive Strength | 70.0 MPa | 10200 psi | Cold Crushing Strength |
Gouda Vuurvast AK 98 Dense Refractory Brick Description: This high alumina brick finds wide application in chemical reactors. The firing temperature of these bricks is very high, which results in an improved thermal shock resistance and bette.. |
|||
Compressive Strength | 70.0 MPa @Time 3.60e+7 sec |
10200 psi @Time 10000 hour |
|
Wolf Kunststoff ZEDEX® ZX-410V7T A4T Polymer Alloy, Fiber Reinforced, Friction Modified Main Characteristics: Fiber-reinforced; Friction-modified; Very high stiffness (higher than that of fiber-reinforced PEEK); Very low thermal expansion coefficient; Low friction; High wear resistance.. |
|||
Compressive Strength | 70.0 MPa | 10200 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |
|||
Compressive Strength | 70.3 MPa | 10200 psi | |
Tra-Con Tra-Bond FS12 Fast Cure Epoxy Adhesive System TRA-BOND FS12 is an epoxy resin formulation developed for room temperature bonding applications where a fast cure epoxy adhesive is needed. This effective epoxy formulation consists of 100% reactive.. |
|||
Compressive Strength | >= 70.0 MPa | >= 10200 psi | Axial; IEC 1212-2 4.2 |
Hippe PF CP 31 Cellulose Paper Reinforced Phenolic Resin - Round, Molded Tube and Rod Used in electrical and mechanical applications. Good stability of electrical properties when exposed to normal relative humidity.Information provided by Hippe. |
|||
Compressive Strength | 70.3 MPa | 10200 psi | |
Aremco Ceramacast™ 576-N High Temperature Potting & Casting Alumina Medium grain castable ceramic for large high temperature potting and tooling. Aremco offers a range of ceramic-based materials used for the assembly of high temperature, high power electrical devic.. |
|||
Compressive Strength | 70.0 MPa @Temperature 200 °C |
10200 psi @Temperature 392 °F |
EN ISO 604 |
Brandenburger S 2000 A Side Insulation S 2000 A is reinforced with load-bearing glass fibre mat with thermoset weave. A laminated aluminum lining provides additional heat-reflecting protection.Information provided by Brandenburger Isolie.. |