Polymer Property : Compressive Strength = 10153 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 70.002 MPa

@Temperature 20.0 °C
10153 psi

@Temperature 68.0 °F
after 7 days
Stellar Canada CERAMITE® CSA Wear Resistant Castable
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w..