Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 2230 - 2430 MPa | 323000 - 352000 psi | Rc0.2; varies with tempering. This range is for HRC between 58 and 61. |
Bohler-Uddeholm UDDEHOLM Caldie Plastic Mold Tool Steel Description: Uddeholm Caldie is a chromium-molybdenumvanadium alloyed tool steel.Uddeholm Caldie which is characterized by:Very good chipping and cracking resistanceGood wear resistanceHigh hardness.. |