Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 210 - 240 MPa | 30500 - 34800 psi | ISO 604 |
Perstorp Compounds Aminel FX Melamine Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp .. |
|||
Compressive Strength | 220 - 240 MPa | 31900 - 34800 psi | ISO 604 |
Vyncolit X681 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction. Tribological compound with PTFE additive.USES: Water pump seals and self-lubrica.. |