Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 200 - 230 MPa | 29000 - 33400 psi | ISO 604 |
Vyncolit 2923 W Novolac Phenolic Mineral filled phenolic molding compound with excellent heat resistance and dimensional stability.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Compressive Strength | 200 - 230 MPa | 29000 - 33400 psi | ISO 604 |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
Compressive Strength | 200 - 230 MPa | 29000 - 33400 psi | ISO 604 |
Vyncolit 2530 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent thermal properties.USES: Lamp sockets, special lamp holders, pan handles and knobs.Information provided by Vyncolit, a Sumitomo Ba.. |
|||
Compressive Strength | 200 - 230 MPa | 29000 - 33400 psi | ISO 604 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Compressive Strength | 200 - 230 MPa | 29000 - 33400 psi | ISO 604 |
Vyncolit 2920 W Novolac Phenolic Mineral and organic filled molding compound with good dimensional stability and heat resistance.USES: Carburettor and intake manifold thermal insulator.Information provided by Vyncolit, a Sumitomo B.. |