Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 9.81 - 19.6 MPa @Temperature 1350 °C, Time 10800 sec |
1420 - 2840 psi @Temperature 2460 °F, Time 3.00 hour |
Cold Crushing Strength |
Chosun Refractories TG-55 Monolithic Refractories for Ladle and Tundish Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |