Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 0.0700 - 0.110 MPa @Strain 40.0 % |
10.2 - 16.0 psi @Strain 40.0 % |
Sponge Silicone Rubber Sheet |
P & P Technology Silicone Sheet Silicone sheet is FDA approved. Translucent sheet is FDA @ WRC approved. FDA Certificate No. 177.2600Information provided by P & P Technology |