Polymer Property : Compressive Strength = 0.0965 MPa
Polymer Property :
Compressive Strength =
0.0965 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Strength
0.0621
-
0.0965
MPa
9.00
-
14.0
psi
0.25; ASTM D1056