Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 827 MPa | 120000 psi | |
Meehanite GE-30 Flake Graphite Cast Iron Type GE-30 combines improved strength and solidity with higher machining feeds and speeds than ordinary gray iron.General Meehanite information - Meehanite metal is first melted to a definite degree.. |
|||
Compressive Strength | 827 MPa | 120000 psi | |
Aremco AREMCOLOX™ 502-676 Machinable Magnesium Oxide Full-fired, fine grain, high purity MgO ceramic. Inert to molten metals, slags, superconductors. Broad line of standard crucibles. Custom parts made to print. |