Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 75.2 MPa | 10900 psi | 2% Def.; ISO 604 |
Quadrant EPP Ketron® 1000 LSG PEEK, Biocompatibility tested (ISO Product Data Sheet) KETRON® PEEK LSG natural / black stock shapes are produced from batches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. .. |
|||
Compressive Strength | 75.2 MPa | 10900 psi | ASTM D-695 |
CMT Materials REN Shape® 472 Machinable Board for Prototype Tooling & Assembly Fixtures RenShape 472 is a polyurethane-based board designed for CNC machining of production grade checking and assembly fixtures. It may also be used in prototype thermoforming and vacuum forming tooling a.. |
|||
Compressive Strength | 75.2 MPa | 10900 psi | |
Abatron AboCast 8103-14 One-Component Epoxy AboCast 8103-14 is the lowest-viscosity one-component epoxy system with heavy-duty structural and dielectric properties. It is clear and has maximum wetting and penetration. Suggested Uses: Casting.. |