Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 65.0 MPa | 9430 psi | Cold Crushing Strength |
Gouda Vuurvast AC 80-5 Dense Refractory Brick Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from.. |
|||
Compressive Strength | 65.0 MPa | 9430 psi | Cold Crushing Strength |
Gouda Vuurvast AK 86 A Dense Refractory Brick Description: This bauxite based brick has a high strength and good erosion resistance. Application in torpedo ladles for the steel industry and outlet zone rotary cement kilns.Remarks: This data rep.. |
|||
Compressive Strength | 65.0 MPa | 9430 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Conditioned Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 65.0 MPa | 9430 psi | 20% pressing; EN ISO 604 |
Schwartz Technical Plastics LAMIGAMID® 300 Cast Polyamide 6, Dry Application: slippers and center blocks for heavy rolling mills, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
Compressive Strength | 65.0 MPa @Temperature 23.0 °C, Time 86400 sec |
9430 psi @Temperature 73.4 °F, Time 24.0 hour |
50% RH, Axial; ISO 604; IEC/EN 61212-2 5.2 |
Elektro-Isola G-Etronax SI Silicone, Glass Fabric Reinforcement, White, Tubes Description: Used in mechanical, electrical and electronic applications at elevated temperatures. Retains good electrical properties at high temperatures. Self-extinguishing. Low dielectric loss fac.. |