Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 573.9 MPa | 83230 psi | Warp; D 6641-01 |
Ensinger TECATEC™ CF60 Polyaryletherketone (PAEK) TECATEC™ CF60 plate is a composite of 60% woven carbon fiber laminated with a polyaryl ether ketone resin (PAEK). It is produced in a proprietary process yielding good fibre and resin integration... |