Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 55.0 MPa | 7980 psi | Cold Crushing Strength |
Gouda Vuurvast AC 80-10 Dense Refractory Brick Description: This bauxite base brick shows, due to the addition of CR2O3, a very good slag resistance.Remarks: This data represents average values, obtained from samples that were cut from standard .. |
|||
Compressive Strength | 55.0 MPa | 7980 psi | Cold Crushing Strength |
Gouda Vuurvast AK 60 M Dense Refractory Brick Description: This quality is produced from high fired raw materials with a high mullite content. The grain distribution for these bricks is carefully selected, so that a maximum density is obtained... |
|||
Compressive Strength | 55.0 MPa | 7980 psi | design compressive strength |
Momentive Performance Materials Type 254 Fused Quartz Tubing A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen .. |
|||
Compressive Strength | 55.0 MPa | 7980 psi | ASTM D695 |
Sumitomo Bakelite North America SI 9045C Silicone Compound Long fiberglass and graphite filled silicone molding compound which offers moderate strength properties, high impact resistance, and excellent thermal stability at elevated temperatures.Information .. |
|||
Compressive Strength | 55.0 MPa | 7980 psi | cured at 725°C |
Pyrotek Pyrocast XL Small Component Refractory ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast.. |