Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 275 MPa | 39900 psi | ISO 604 |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ISO 604 |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-4-220BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-4-222NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-222NA 40% glass fiber reinforced polyphenylene sulfide compound provides enhanced mechanical strength after constant or repeated exposure to high temperature water and complies with Un.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-4-230NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-4-232NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-232NA 40% glass fiber reinforced polyphenylene sulfide compound complies with United States Food and Drug Administration (FDA) and European Union (EU 10/2011 and 1183/2012) regulations.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-7-190BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190BL glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-7-190NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-190NA glass fiber and mineral filled polyphenylene sulfide compound provides enhanced strength and low maintenance molding using conventional molding equipment.Features: Good Chemical .. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM D695 |
Solvay Specialty Polymers Ryton® R-4-220NA Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-220NA and R-4-220BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength after constant or repeated exposure to high temperature water.Featur.. |
|||
Compressive Strength | 275 MPa | 39900 psi | ISO 604 |
Vyncolit X640 Resole Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Compressive Strength | >= 275 MPa | >= 39900 psi | Perpendicular to laminations; IEC 1212-2 5.3 |
Hippe MF GC 201 Woven Glass Cloth Reinforced Melamine Resin - Sheet Used in mechanical and electrical applications. High mechanical strength. Arc and tracking resistant. Flame retardant. Information provided by Hippe. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM C773-88 |
CeramTec 547 Cordierite (2MgO-2Al2O3-5SiO2) Te value is 670°C. Hasselman Thermal Shock value is 800 K.Data provided by CeramTec North America. |
|||
Compressive Strength | 275 MPa | 39900 psi | ASTM C-773-88 / DIN 51067T1 |
CeramTec GRADE A LAVA Machinable Ceramic GRADE A LAVA is a machineable ceramic that exhibits good electrical and heat resistance. It is excellent in applications where close tolerances must be held. This material is available in a variety .. |