Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 240 MPa
34800 psi
ISO 604
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy  (discontinued **)
Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha..
Compressive Strength 240 MPa
34800 psi
ASTM D695
Sumitomo Bakelite North America E 2748-9641D Short Glass Fiber Reinforced Epoxy
E 2748-9641D is a mineral and short fiberglass filled epoxy molding compound.Information provided by Sumitomo Bak North America, Inc.
Compressive Strength 240 MPa
34800 psi
ASTM D695
Sumitomo Bakelite North America E 8940SG Electrical Encapsulation Grade Epoxy
Mineral reinforced epoxy molding compound formulated for the encapsulation of electronic devices requiring high quality, exceptional reliability, and outstanding moldability. USES: Passive electron..
Compressive Strength 240 MPa
34800 psi
ASTM D695
Sumitomo Bakelite North America Epiall® 1908-1 Short Glass Fiber Reinforced Epoxy
Epiall 1908-1 is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation proper-ties that meets the requir..
Compressive Strength 240 MPa
34800 psi
ISO 604
Vyncolit 4421 XB Novolac Phenolic
Mineral and organic filled phenolic molding compound with good mechanical properties.USES: Fuse holders, brush holders, circuit breakers, automotive ignition and solenoid covers.Information provided..
Compressive Strength 240 MPa

@Thickness >=5.00 mm
34800 psi

@Thickness >=0.197 in
24hr/23°C/50% RH; ISO 604; IEC/EN 60893-2 5.3
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..
Compressive Strength 240 MPa
34800 psi
ASTM D695
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)
Tecapeek™, made from Victrex® PEEK polymer, is an excellent material for a wide spectrum of applications where thermal, chemical, and combustion properties are critical to performance. Excellent ..
Compressive Strength 240 MPa

@Temperature 22.8 °C
34800 psi

@Temperature 73.0 °F
ASTM D695
Ensinger Tecapeek® MT CF 30 Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..
Compressive Strength 240 - 280 MPa
34800 - 40600 psi
ISO 604
Vyncolit X682 Novolac Phenolic
Glass fiber, glass bead and graphite filled phenolic molding compound with excellent mechanical properties and a low coefficient of friction.USES: Water pump seals and self-lubricating bearings.Info..
Compressive Strength 240 MPa
34800 psi
ASTM D695
Resinoid 1360 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Compressive Strength 240 MPa
34800 psi
ASTM D695
Ensinger Sintimid™ ESD 23 Polyamide-imide (PAI)  (discontinued **)
SINTIMID™ ESD 23 has the highest compressive strength and use temperature of the group. It is based on an Ensinger-Hyde manufactured polyamide-imide resin with a low sloughing, additive package.In..
Compressive Strength 240 MPa
34800 psi
ASTM D695
Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information ..
Compressive Strength 240 MPa
34800 psi
ASTM D695
Sumitomo Bakelite North America FM 4008 Fiberglass and Mineral Reinforced Phenolic Resole
FM 4008 is a fiberglass and mineral reinforced phenolic resole compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North A..