Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 234 MPa | 33900 psi | ASTM D695 |
Resinoid 1363 Phenolic Molding, Glass Reinforced Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance |
|||
Compressive Strength | 234 MPa | 33900 psi | ASTM D695 |
IDI Composites 46-16-60 Thermoset Polyester, Sheet TRANSIT - A premium molding compound with excellent resistance to flame and smoke generation, high impact strength, and weatherability.Data provided by the manufacturer. |
|||
Compressive Strength | 234 MPa | 33900 psi | ASTM D695 |
IDI Composites C-210 Thermoset Polyester, Sheet CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by .. |
|||
Compressive Strength | 234 MPa | 33900 psi | ASTM D695 |
IDI Composites E-207 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Compressive Strength | 234 MPa @Thickness 12.7 mm |
34000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP310 Cotton Fabric Description: Canvas machining grade for structural and mechanical applications. Better impact strength than phenolic paper grades. MIL-I-24768/16. Thickness Tested: 0.062, 0.125", and 0.500". |
|||
Compressive Strength | 234 MPa @Thickness 12.7 mm |
34000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP310E Cotton Fabric Description: Manufactured with a domestic cotton fabric and phenolic resin. Similar to NP310 with improved moisture resistance and electrical properties. Mechanical properties equivalent to NP310. M.. |
|||
Compressive Strength | 234 MPa @Thickness 12.7 mm |
34000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP329 Cotton Fabric Description: Bleached linen with melamine resin system. Provides better arc resistance than NP320E. Also, resistant to ammonia based refrigerants. Hard, durable material should be heated to punch, .. |
|||
Compressive Strength | 234 MPa | 33900 psi | |
Momentive Performance Materials Boralloy® PBN Pyrolytic Boron Nitride Boralloy® Pyrolytic Boron Nitride (PBN) is an anisotropic, high-temperature ceramic which exhibits a unique combination of high electrical resistance and good thermal conductivity. This non-toxi.. |
|||
Compressive Strength | 234 MPa | 33900 psi | |
Haysite H258 Polyester Laminate Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications.. |
|||
Compressive Strength | 234 MPa | 33900 psi | |
Haysite H260 Polyester Laminate Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet m.. |
|||
Compressive Strength | 234 MPa | 33900 psi | ASTM D695 |
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro.. |
|||
Compressive Strength | 234 - 241 MPa | 34000 - 35000 psi | |
Bulk Molding Compounds BMC 1608 Very High Strength, Corrosion Resistant BMC 1608 is a very high strength, general purpose, corrosion resistant material. Recommended for compression molding only. UL® recognized. Meets FDA requirements for food contact. This material was.. |
|||
Compressive Strength | 234 MPa @Thickness 12.7 mm |
34000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **) Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f.. |