Mechanical Properties Metric English Comments
Compressive Strength 2250 MPa
326000 psi
HRC 62 R<sub>c</sub>0.2
Assab Steels DF-3 Cold Work Steel
DF-3 general purpose oil-hardening tool steel is a versatile manganese-chromium-tungsten steel suitable for a wide variety of cold-work applications. Its main characteristics include:Good machinabil..