Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 221 MPa | 32000 psi | |
Mykroy/Mycalex MM 600 Machining Grade Glass-bonded Mica Composite Formerly known as grade MM 1100. Synthetic mica filler. Does not burn. Excellent radiation resistance (3 x 10^10 Rads-Cobalt).This ceramoplastic material is a versatile and efficient insulating m.. |
|||
Compressive Strength | 221 MPa | 32000 psi | 10% Def.; ASTM D695 |
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet) |
|||
Compressive Strength | 221 MPa | 32100 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Compressive Strength | 221 MPa | 32100 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI)
(Unverified Data**) Torlon 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon PAI has the hi.. |
|||
Compressive Strength | 221 MPa @Thickness 12.7 mm |
32000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP842 Paper Base Laminate
(discontinued **) Description: Paper reinforced phenolic grade with controlled conductivity. Mechanical strength similar to NP611. NP842 is semi-conductive on the surfaces and through the laminate.Thickness Tested: 0.. |
|||
Compressive Strength | 221 MPa | 32100 psi | ASTM D695 |
IDI Composites A-207 Thermoset Polyester, Sheet AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r.. |
|||
Compressive Strength | 221 MPa | 32100 psi | ASTM D695 |
IDI Composites E-206 Thermoset Polyester, Sheet ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista.. |
|||
Compressive Strength | 221 MPa | 32100 psi | ASTM D695 |
IDI Composites M-207 Thermoset Polyester, Sheet MECHANICAL - Versatile family of compounds designed to meet a variety of mechanical, electro-mechanical, and corrosion applications. Outstanding structural properties at lowest possible costs.Data p.. |
|||
Compressive Strength | 221 MPa @Thickness 12.7 mm |
32000 psi @Thickness 0.500 in |
ASTM D695 |
Industrial Laminates/Norplex NP193E Synthetic Fabric Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temp.. |
|||
Compressive Strength | 221 MPa @Thickness 12.7 mm |
32000 psi @Thickness 0.500 in |
Flatwise |
Industrial Laminates/Norplex NP631 Paper Base Laminate Description: Hot punching grade with excellent electrical properties and low moisture absorption.Thickness Tested: 0.062", 0.125" and 0.500" |
|||
Compressive Strength | 221 MPa | 32000 psi | ASTM D695 |
Haysite H722 Polyester, Glass Reinforced H722 is an all-purpose GPO-1 fiberglass mat reinforced thermoset polyester molded sheet. Available in thicknesses ranging from .031" - 2.00". Standard color - Natural. Meets Gov't Specs - LP-509, .. |
|||
Compressive Strength | 221 MPa | 32100 psi | |
Haysite HCR-191 Corrosion Resistant Polyester/Glass Sheet A fiber glass reinforced thermoset sheet using HETRON 197® flame resistant polyester in the resin matrix. Standard color is light beige. Additional data covering resistance to specific chemicals .. |
|||
Compressive Strength | 221 MPa | 32000 psi | |
SGL Carbon Group EK 200 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 221 MPa | 32000 psi | |
SGL Carbon Group EK 201 Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Compressive Strength | 221 MPa | 32100 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI) Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic.. |
|||
Compressive Strength | 221 MPa | 32100 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4203L Polyamide-imide (PAI) Torlon® 4203L is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin. It has the best impact resistance and greatest elongation of all the Torlon® grades. Torlon® PA.. |
|||
Compressive Strength | 221 MPa | 32100 psi | ASTM D695 |
Sumitomo Bakelite Durez® 31906 Phenolic, Injection Grade Durez 31906 Black Phenolic is an asbestos free, medium impact, molding compound. It is designed for applications where additional mechanical strength is required.Information provided by Sumitomo Ba.. |
|||
Compressive Strength | <= 221 MPa | <= 32000 psi | ASTM D695 |
Ensinger Tecapeek® XP-95 Compression Molded PEEK Compound, 15% PTFE Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Compressive Strength | 221 MPa | 32000 psi | |
Aremco AREMCOLOX™ 502-600 Machinable Glass Ceramic High dielectric and mechanical strength. For high voltage insulators, lamp housings, thermal switches, and radiation parts. Readily machined, no firing required. Plates from 1/8" to 1" thick; rod.. |
|||
Compressive Strength | 221 MPa | 32100 psi | ASTM D695 |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |
|||
Compressive Strength | 221 MPa | 32100 psi | |