Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 22.8 MPa | 3300 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® 1000 EC Electrically Conductive UHMW (ASTM Product Data Sheet) |
|||
Compressive Strength | 22.8 MPa | 3300 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® 1000 UV Stabilized UHMW, Black (ASTM Product Data Sheet) |
|||
Compressive Strength | 22.8 MPa | 3300 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet) |
|||
Compressive Strength | 22.8 MPa | 3300 psi | 10% Def.; ASTM D695 |
Quadrant EPP TIVAR® ESD Electro Static Dissipative UHMW-PE (ASTM Product Data Sheet) Protects against electrical charge build-up Reduces noise Self-lubricating Corrosion-resistant No moisture absorption |
|||
Compressive Strength | 22.8 MPa | 3300 psi | 1% strain; ASTM D695 |
Saint-Gobain Meldin® 7001 Isostatically Molded Polyimide Finished parts and basic shapes made from unfilled polyimide material for structural applications requiring requiring high electrical insulative properties, high purity and low outgassing, and high .. |
|||
Compressive Strength | 22.8 MPa | 3300 psi | 1% strain; ASTM D695 |
Saint-Gobain Meldin® 7211 Isostatically Molded Graphite and PTFE Filled Polyimide Finished parts and basic shapes made from 10% by weight PTFE and 15% by weight graphite filled polyimide material for applications requiring a very low coefficient of friction and self-lubricating p.. |