Polymer Property : Compressive Strength = 213 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 213 MPa
30900 psi
ASTM D695
Sumitomo Bakelite North America E 3812M-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
E 3812M-1 is a mineral and short fiberglass filled epoxy molding compound for low pressure encapsulation molding, featuring excellent dimensional stability, good thermal shock resistance, and good e..
Compressive Strength 213 MPa
30900 psi
ASTM D695
Plenco 2408 Phenolic, Granular, Injection Molded
PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi..